Wood shrinkage rate properties

Wood shrinkage rate properties: string to 4.4 % ~ 8.3%; radial 2.4%. timber weight; air-dry density 0.83gcm3); strength of medium to high; parallel to grain compressive strength 60MPa, bending strength 106MPa, flexural modulus 14GPa. decay. Drying difficult, quite slow. processing difficult. timber suitable for making use of the floor; also suitable for production of water in the piles, bridges, piers, building construction, interior decoration. the name of breast milk mulberry mulberry wood, Bagasse spp., bagasse, tatajuba; scribe legumes, milk Morus. common milk product Herve Leger timber mainly Guyana Sang B.guianensis, the market misleading name: Kim Nan, Yulan, South America, cinnamon wood. trees and distribution of large trees, no board root;
high 27 ~ 30m; round straight trunk, canopy height 18 ~ 21m; diameter 60 ~ 95cm; bark can be out of a lot of sticky milk. is mainly produced in northern South America. red ant red ant wood wood name, Tabebuia spp; roble, mayflower, amapa; scribe Zi Wei Ke, ants are wood, red wood ant. red wood ant. common commercial timber of red ants are mainly wood T.rosea, gray termites and other wood T.pallida. trees and the distribution of trees, short board root 2 ~ 3m ; stem form often irregular, high 12 ~ 18m, up 27m, diameter 46 ~ 60cm, there are up to 90cm. is mainly produced in Mexico, the West Indies south to Venezuela and Ecuador.

No comments:

Post a Comment